Spiral fracture in metallic glasses and its correlation with failure criterion
Lei XQ(雷现奇); Wei YJ(魏宇杰); Wei BC(魏炳忱); Wang WH(汪卫华); Wei, YJ (reprint author), Chinese Acad Sci, Inst Mech, LNM, Beijing 100190, Peoples R China.
发表期刊ACTA MATERIALIA
2015-10-15
卷号99页码:206-212
ISSN1359-6454
摘要We report the observation of spiral fracture of the metallic glass Zr41Ti14Cu12.5Ni10Be22.5 (at.%) subjected to both shear and normal stresses. The spiral angle (that between the spiral line and the loading axis) increases as we gradually change the normal stress from tensile (positive) to compressive (negative). The spiral nature of the fractured surface leads to a left-handed helix fractography pattern in tension, and a right-handed helix in compression. The Mohr Coulomb type of failure is essential for the unique spiral fracture. The use of spiral angles resulted from torsion tension experiments provide another novel experimental strategy to examine the failure criterion as well as stress state dependence of deformation mechanisms which lead to failure in metallic glasses. (C) 2015 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
关键词Metallic Glasses Failure Criterion Mohr-coulomb Spiral Fracture
DOI10.1016/j.actamat.2015.08.008
URL查看原文
收录类别SCI ; EI
语种英语
WOS记录号WOS:000362145400022
关键词[WOS]HYDROSTATIC-PRESSURE ; MECHANICAL-BEHAVIOR ; AMORPHOUS-ALLOYS ; YIELD CRITERION ; DEFORMATION ; FLOW ; INDENTATION ; STRAIN ; LOCALIZATION ; COMPRESSION
WOS研究方向Materials Science ; Metallurgy & Metallurgical Engineering
WOS类目Materials Science, Multidisciplinary ; Metallurgy & Metallurgical Engineering
项目资助者The authors acknowledge support from National Natural Science Foundation of China (NSFC) (11425211, 11021262, 11272327), MOST 973 of China (2012CB937500). The authors are grateful to Prof. J. Lewandowski and Prof. A. Lindsay Greer for fruitful discussion.
课题组名称LNM微结构计算力学(筹)
论文分区一类
引用统计
被引频次:25[WOS]   [WOS记录]     [WOS相关记录]
文献类型期刊论文
条目标识符http://dspace.imech.ac.cn/handle/311007/58409
专题非线性力学国家重点实验室
通讯作者Wei, YJ (reprint author), Chinese Acad Sci, Inst Mech, LNM, Beijing 100190, Peoples R China.
推荐引用方式
GB/T 7714
Lei XQ,Wei YJ,Wei BC,et al. Spiral fracture in metallic glasses and its correlation with failure criterion[J]. ACTA MATERIALIA,2015,99:206-212.
APA Lei XQ,Wei YJ,Wei BC,Wang WH,&Wei, YJ .(2015).Spiral fracture in metallic glasses and its correlation with failure criterion.ACTA MATERIALIA,99,206-212.
MLA Lei XQ,et al."Spiral fracture in metallic glasses and its correlation with failure criterion".ACTA MATERIALIA 99(2015):206-212.
条目包含的文件 下载所有文件
文件名称/大小 文献类型 版本类型 开放类型 使用许可
J2015-051.pdf(1311KB)期刊论文作者接受稿开放获取CC BY-NC-SA浏览 下载
个性服务
推荐该条目
保存到收藏夹
查看访问统计
导出为Endnote文件
Lanfanshu学术
Lanfanshu学术中相似的文章
[Lei XQ(雷现奇)]的文章
[Wei YJ(魏宇杰)]的文章
[Wei BC(魏炳忱)]的文章
百度学术
百度学术中相似的文章
[Lei XQ(雷现奇)]的文章
[Wei YJ(魏宇杰)]的文章
[Wei BC(魏炳忱)]的文章
必应学术
必应学术中相似的文章
[Lei XQ(雷现奇)]的文章
[Wei YJ(魏宇杰)]的文章
[Wei BC(魏炳忱)]的文章
相关权益政策
暂无数据
收藏/分享
文件名: J2015-051.pdf
格式: Adobe PDF
所有评论 (0)
暂无评论
 

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。