Peeling Experiments Of Ductile Thin Films Along Ceramic Substrates - Critical Assessment Of Analytical Models 期刊论文
International Journal of Solids and Structures, 2008, 页码: 3779-3792
Authors:  Wei YG(魏悦广);  Zhao HF(赵海峰);  Wei, YG (reprint author), Chinese Acad Sci, Inst Mech, LNM, Beijing 100080, Peoples R China.
Adobe PDF(867Kb)  |  Favorite  |  View/Download:712/165  |  Submit date:2009/08/03
Peel Experiment  Metal Thin Film  Analytical Model  Interfacial Fracture Energy  Pressure-sensitive Adhesive  Strain Gradient Plasticity  State Crack-growth  Fracture Criterion  Cantilever Beam  Round-robin  Work  Toughness  Strength  Surface  
On The Cyclic Bending Behaviour Of A Hard Coating On A Ductile Substrate With Periodic Surface Hardened Regions 期刊论文
International Journal of Solids and Structures, 2008, 页码: 5661-5674
Authors:  Wu CW(吴臣武);  Zhang K(张坤);  Chen GN(陈光南);  Wu, CW (reprint author), Chinese Acad Sci, Inst Mech, 15 Beisihuanxi Rd, Beijing 100190, Peoples R China.
Adobe PDF(1713Kb)  |  Favorite  |  View/Download:871/187  |  Submit date:2009/08/03
Hard Coating  Ductile Substrate  Periodic Surface Hardened Regions  Cyclic Bending  Interface Fracture  Subsurface Inclusions  Segmentation Cracks  Steel Substrate  Indentation  Stresses  Fracture  Design