Crack initiation behavior and fatigue performance up to very-high-cycle regime of AlSi10Mg fabricated by selective laser melting with two powder sizes 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2021, 卷号: 143, 页码: 12
Authors:  Jian ZM(渐徵墨);  Qian GA(钱桂安);  Paolino, D. S.;  Tridello, A.;  Berto, F.;  Hong YS(洪友士)
Adobe PDF(12679Kb)  |  Favorite  |  View/Download:381/75  |  Submit date:2021/03/03
Selective laser melting  AlSi10Mg  VHCF  Defects  Crack initiation  
Effects of inclusion size and stress ratio on the very-high-cycle fatigue behavior of pearlitic steel 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2021, 卷号: 142, 页码: 11
Authors:  Cong, Tao;  Qian, Guian;  Zhang, Guanzhen;  Wu, Si;  Pan, Xiangnan;  Du, Leiming;  Liu, Xiaolong
Adobe PDF(13962Kb)  |  Favorite  |  View/Download:256/53  |  Submit date:2021/01/12
Pearlitic steel  Very-high-cycle fatigue  Inclusion size  Stress ratio  Nanograins