In-situ investigation on fatigue behaviors of Ti-6Al-4V manufactured by selective laser melting 会议论文
19th International Colloquium on Mechanical Fatigue of Metals (ICMFM), Univ Porto, Fac Engn, Porto, PORTUGAL, SEP 05-07, 2018
作者:  Qian GA(钱桂安);  Jian,Zhimo;  Pan XN(潘向南);  Berto,Filippo
Adobe PDF(2875Kb)  |  收藏  |  浏览/下载:106/37  |  提交时间:2022/11/24
Selective laser melting  In-situ SEM  Ti-6Al-4V  Low cycle fatigue  Crack propagation  
The behavior of crack initiation and early growth in high-cycle and very-high-cycle fatigue regimes for a titanium alloy 会议论文
4th IJFatigue and FFEMS Joint Workshop on Characterisation of Crack Tip Fields, Bonifacio, FRANCE, APR 10-12, 2017
作者:  Pan XN(潘向南);  Su H(苏杭);  Sun CQ(孙成奇);  Hong YS(洪友士)
浏览  |  Adobe PDF(6409Kb)  |  收藏  |  浏览/下载:376/60  |  提交时间:2019/04/19
Very-high-cycle fatigue  Crack initiation  Mean stress  Titanium alloy  Equiaxed microstructure  
The formation mechanism of characteristic region at crack initiation for very-high-cycle fatigue of high-strength steels 会议论文
3rd International Conference on Characterisation of Crack Tip Fields, Urbino, ITALY, APR 20-22, 2015
作者:  Hong YS(洪友士);  Liu XL(刘小龙);  Lei ZQ(雷铮强);  Sun CQ(孙成奇);  Hong, YS (reprint author), Chinese Acad Sci, Inst Mech, LNM, Beijing 100190, Peoples R China.
浏览  |  Adobe PDF(3960Kb)  |  收藏  |  浏览/下载:336/107  |  提交时间:2017/05/12
Very-high-cycle Fatigue  Fatigue Crack Initiation  Fine-granular-area  Nanograins  High-strength Steels  Chromium-bearing Steel  Long-life Fatigue  N-greater-than-10(7) Cycles  Residual-stresses  Vhcf-regime  Behavior  Inclusions  Propagation  Damage  Size