In-situ investigation on fatigue behaviors of Ti-6Al-4V manufactured by selective laser melting 会议论文
19th International Colloquium on Mechanical Fatigue of Metals (ICMFM), Univ Porto, Fac Engn, Porto, PORTUGAL, SEP 05-07, 2018
作者:  Qian GA(钱桂安);  Jian,Zhimo;  Pan XN(潘向南);  Berto,Filippo
Adobe PDF(2875Kb)  |  收藏  |  浏览/下载:106/37  |  提交时间:2022/11/24
Selective laser melting  In-situ SEM  Ti-6Al-4V  Low cycle fatigue  Crack propagation  
Faceted crack initiation characteristics for high-cycle and very-high-cycle fatigue of a titanium alloy under different stress ratios 会议论文
5th International Conference on Crack Paths (CP), Ferrara, ITALY, SEP, 2015
作者:  Liu XL(刘小龙);  Sun CQ(孙成奇);  Hong YS(洪友士);  Hong, YS (reprint author), Chinese Acad Sci, Inst Mech, LNM, Beijing 100190, Peoples R China.
浏览  |  Adobe PDF(2579Kb)  |  收藏  |  浏览/下载:383/77  |  提交时间:2017/05/12
Ti-6al-4v Alloy  Faceted Crack Initiation  Very-high-cycle Fatigue  Stress Ratio  Cluster Of Primary Alpha Grains  Competing Failure Modes  Poisson Defect Statistics  Ti-6al-4v Alloy  Structural-materials  Mean Stress  Strength  Microstructure  Behavior  Duality  Surface  
Intrinsic lengths govern failure mode transition in metallic glasses 会议论文
ICTAM, 北京, 2012-8
作者:  Dai LH(戴兰宏);  Chen Y(陈艳)
Adobe PDF(691Kb)  |  收藏  |  浏览/下载:1780/1224  |  提交时间:2013/03/01
First principles based predictions of the toughness of a metal/oxide interface 会议论文
7th International Workshop on Interfaces - New materials Via Interfacial Control, Santiago de Compostela, SPAIN, JUN 22-26, 2008
作者:  Jiang Y;  Wei YG(魏悦广);  Smith JR;  Hutchinson JW;  Evans AG
Adobe PDF(1249Kb)  |  收藏  |  浏览/下载:886/190  |  提交时间:2009/07/23
Toughness  Interface  Density Functional Theory  Multi-scale Modeling  Cohesive Zone  Thermal Barrier Systems  Plasticity  Decohesion  Separation  Adhesion  Ni/al2o3