Fatigue life prediction for LPBF-fabricated Ti-6Al-4V up to very-high-cycle regime based on continuum damage mechanics incorporating effect of defects 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2024, 卷号: 181, 页码: 13
作者:  Ling, Chao;  Jia, Yinfeng;  Fu, Rui;  Zheng, Liang;  Zhong, Zheng;  Hong YS(洪友士)
收藏  |  浏览/下载:20/0  |  提交时间:2024/03/11
Fatigue life prediction  LPBF-fabricated Ti-6Al-4V  Continuum damage mechanics  Defect  Very-high-cycle fatigue  
Effects of loading frequency on fatigue behavior of metallic materials-A literature review 期刊论文
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2023
作者:  Hong YS(洪友士);  Hu, Yuanpei;  Zhao, Aiguo
Adobe PDF(4219Kb)  |  收藏  |  浏览/下载:58/0  |  提交时间:2023/06/15
fatigue strength  loading frequency  metallic materials  strain rate  very-high-cycle fatigue  
An experimental investigation of fatigue performance and crack initiation characteristics for an SLMed Ti-6Al-4V under different stress ratios up to very-high-cycle regime 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2022, 卷号: 164, 页码: 14
作者:  Fu, Rui;  Zheng, Liang;  Ling, Chao;  Zhong, Zheng;  Hong YS(洪友士)
Adobe PDF(26974Kb)  |  收藏  |  浏览/下载:249/35  |  提交时间:2022/08/28
Selective laser melting  Ti-6Al-4V  Very-high-cycle fatigue  Crack initiation  Stress intensity factor  
Multiaxial fatigue life prediction by equivalent energy-based critical plane damage parameter under variable amplitude loading 期刊论文
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2022
作者:  Tao ZQ(陶志强);  Qian GA(钱桂安);  Sun JY(孙经雨);  Zhang ZL;  Hong YS(洪友士)
Adobe PDF(7297Kb)  |  收藏  |  浏览/下载:117/34  |  提交时间:2022/10/23
critical plane  damage parameter  life prediction  multiaxial fatigue  variable amplitude loading  
再论超高周疲劳裂纹萌生特征区 期刊论文
力学学报, 2022, 卷号: 54, 期号: 08, 页码: 2101-2118
作者:  洪友士
Adobe PDF(2119Kb)  |  收藏  |  浏览/下载:136/46  |  提交时间:2022/11/14
超高周疲劳  裂纹萌生  特征区  高强钢  钛合金  
Crack initiation mechanisms under two stress ratios up to very-high-cycle fatigue regime for a selective laser melted Ti-6Al-4V 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2021, 卷号: 149, 页码: 10
作者:  Du LM(杜雷鸣);  Pan XN(潘向南);  Qian GA(钱桂安);  Zheng L(郑亮);  Hong YS(洪友士)
Adobe PDF(14294Kb)  |  收藏  |  浏览/下载:281/54  |  提交时间:2021/08/03
Very-high-cycle fatigue  Crack initiation mechanism  Stress ratio  Ti-6Al-4V  Selective laser melting  
Guest editorial: Characterisation of crack tip fields-CCTF5 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2020, 卷号: 140, 页码: 1
作者:  Vormwald M;  James N;  Hong YS(洪友士);  Susmel L;  Iacoviello F
Adobe PDF(234Kb)  |  收藏  |  浏览/下载:218/42  |  提交时间:2020/10/23
Influence of processing parameters of selective laser melting on high-cycle and very-high-cycle fatigue behaviour of Ti-6Al-4V 期刊论文
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2020, 页码: 17
作者:  Du LM(杜雷鸣);  Qian GA(钱桂安);  Zheng L;  Hong YS(洪友士)
Adobe PDF(52217Kb)  |  收藏  |  浏览/下载:302/98  |  提交时间:2020/11/30
orthogonal experiment design  processing parameters  selective laser melting  Ti-6Al-4V  very-high-cycle fatigue  
Very-high-cycle fatigue behavior of AlSi10Mg manufactured by selective laser melting: Effect of build orientation and mean stress 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2020, 卷号: 138, 页码: 9
作者:  Qian GA(钱桂安);  Jian ZM;  Qian YJ;  Pan XN(潘向南);  Ma XF;  Hong YS(洪友士)
Adobe PDF(11591Kb)  |  收藏  |  浏览/下载:382/175  |  提交时间:2020/08/26
Selective laser melting  Very-high-cycle fatigue  AlSi10Mg  Crack initiation  Fatigue strength  
The mechanism of internal fatigue-crack initiation and early growth in a titanium alloy with lamellar and equiaxed microstructure 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 卷号: 798, 页码: 140110
作者:  Pan XN(潘向南);  Xu SW(徐守文);  Qian GA(钱桂安);  Alexander N;  Andrey S;  Thierry PL;  Hong YS(洪友士)
Adobe PDF(27976Kb)  |  收藏  |  浏览/下载:516/98  |  提交时间:2020/08/26