The Evolution of Micromechanical Properties for Zr-Based Metallic Glass Induced by Laser Shock Peening 期刊论文
FRONTIERS IN MATERIALS, 2021, 卷号: 8, 页码: 6
作者:  Li YS(李炎森);  Wang, Zhitao;  Wei YP(魏延鹏);  Chen TY(陈天宇);  Zhang, Chunfeng;  Huan Y(郇勇);  Zhang K(张坤);  Wei BC(魏炳忱)
Adobe PDF(2123Kb)  |  收藏  |  浏览/下载:263/36  |  提交时间:2022/01/24
metallic glass  laser shock peening  nanoindentation  serrations  micromechanical properties  
The formation of discontinuous gradient regimes during crack initiation in high strength steels under very high cycle fatigue 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2019, 卷号: 124, 页码: 483-492
作者:  Sun CQ(孙成奇);  Zhou LL(周玲玲);  Liu JL;  Wang Y(王垚);  Wu XL(武晓雷);  Wei YJ(魏宇杰)
浏览  |  Adobe PDF(8304Kb)  |  收藏  |  浏览/下载:322/133  |  提交时间:2019/09/09
Very high cycle fatigue  Gradient microstructure  Mechanism of crack initiation  Crack growth rate  
Characteristic of interior crack initiation and early growth for high cycle and very high cycle fatigue of a martensitic stainless steel 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 卷号: 758, 页码: 112-120
作者:  孙成奇i;  Song QY(宋庆元);  Zhou LL(周玲玲);  Pan XN(潘向南)
浏览  |  Adobe PDF(5866Kb)  |  收藏  |  浏览/下载:339/91  |  提交时间:2019/09/09
Very high cycle fatigue  Crack initiation  Crack growth rate  Grain refinement  Multi-site crack initiation  
Comparison of TCD and SED methods in fatigue lifetime assessment 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2019, 卷号: 123, 页码: 105-134
作者:  Hu Z;  Berto F;  Hong YS(洪友士);  Susmel L
浏览  |  Adobe PDF(6308Kb)  |  收藏  |  浏览/下载:256/66  |  提交时间:2019/05/29
Theory of Critical Distances  Strain Energy Density  Modified Wohler Curve  Uniaxial fatigue  Multiaxial fatigue