IMECH-IR

浏览/检索结果: 共44条,第1-10条 帮助

限定条件    
已选(0)清除 条数/页:   排序方式:
Synthesis and characterization of light-weight porous ceramics used in the transpiration cooling 期刊论文
ACTA ASTRONAUTICA, 2020, 卷号: 177, 页码: 438-445
作者:  Zhang, Bo;  Huang, Jie;  Li, Weijie;  Huang, Haiming;  Zhao, Huanyu;  Peng JL(彭锦龙)
Adobe PDF(8097Kb)  |  收藏  |  浏览/下载:373/70  |  提交时间:2021/03/30
Carbon fiber-reinforced silicon carbide porous ceramics  Permeability  Oxyacetylene flame test  Transpiration cooling  
选区激光熔化成形高强高韧316L不锈钢工艺及力学性能研究 学位论文
博士论文,北京: 中国科学院大学, 2020
作者:  蒋华臻
Adobe PDF(56605Kb)  |  收藏  |  浏览/下载:535/16  |  提交时间:2021/01/19
增材制造  选区激光熔化  无量纲工艺图  力学性能  316L不锈钢  
高熵合金在极端条件下的塑性流动行为 学位论文
博士论文,北京: 中国科学院大学, 2020
作者:  蒲卓
Adobe PDF(9778Kb)  |  收藏  |  浏览/下载:1149/37  |  提交时间:2021/01/15
高熵合金,氢脆,极低温,准等熵加载,大塑性变形  
Crack initiation mechanism and fatigue life of titanium alloy Ti-6Al-2Sn-2Zr-3Mo-X: Effects of stress ratio and loading frequency 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 卷号: 798, 页码: 140265
作者:  Sun CQ(孙成奇);  Li YQ;  Huang RX;  Wang L;  Liu JL;  Zhou LL(周玲玲);  Duan GH(段桂花)
Adobe PDF(20240Kb)  |  收藏  |  浏览/下载:253/67  |  提交时间:2020/12/28
Ti-6Al-2Sn-2Zr-3Mo-X  HIGH-CYCLE FATIGUE  Stress ratio  TI-6AL-4V  Frequency  ALPHA  Crack initiation mechanism  BEHAVIOR  Fatigue life  FAILURE  MICROSTRUCTURE  STRENGTH  SIZE  
Damage modeling of oxide/oxide ceramic matrix composites under cyclic loading conditions 期刊论文
CERAMICS INTERNATIONAL, 2020, 卷号: 46, 期号: 15, 页码: 23379-23389
作者:  Liu H;  Yuan H;  Yang ZM(杨正茂)
Adobe PDF(8663Kb)  |  收藏  |  浏览/下载:320/74  |  提交时间:2020/10/29
Oxide/oxide ceramic matrix composite  Continuum damage model  Elastic-plastic damage  Cyclic loading  
Effect of Process Parameters on Defects, Melt Pool Shape, Microstructure, and Tensile Behavior of 316L Stainless Steel Produced by Selective Laser Melting 期刊论文
ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2020, 页码: 16
作者:  Jiang HZ(蒋华臻);  Li ZY(李正阳);  Feng T;  Wu PY;  Chen QS(陈启生);  Feng YL;  Chen LF;  Hou JY(侯静宇);  Xu HJ
Adobe PDF(6860Kb)  |  收藏  |  浏览/下载:388/77  |  提交时间:2020/11/30
Selective laser melting  Defects  Melt pool shape  Primary dendrite spacing  Mechanical properties  316L stainless steel  
Preface to the viewpoint set on: Heterogeneous gradient and laminated materials 期刊论文
SCRIPTA MATERIALIA, 2020, 卷号: 187, 页码: 307-308
作者:  Lu L;  Wu XL(武晓雷);  Beyerlein Iene J
Adobe PDF(224Kb)  |  收藏  |  浏览/下载:225/92  |  提交时间:2020/08/26
Heterogeneous  Gradient and laminated materials  
Fatigue short crack propagation behavior of selective laser melted Inconel 718 alloy by in-situ SEM study: Influence of orientation and temperature 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2020, 卷号: 139, 页码: 14
作者:  Ma X F;  Zhai H L;  Zuo L;  Zhang W J;  Rui S S;  Han Q N;  Jiang J S;  Li C P;  Chen G F;  Qian GA(钱桂安);  Zhao S J
Adobe PDF(8380Kb)  |  收藏  |  浏览/下载:301/143  |  提交时间:2020/08/26
Inconel 718  Selective laser melting  Microstructure  Fatigue short crack growth  In-situ SEM  
Probabilistic framework for fatigue life assessment of notched components under size effects 期刊论文
INTERNATIONAL JOURNAL OF MECHANICAL SCIENCES, 2020, 卷号: 181, 页码: 12
作者:  Liao D;  Zhu SP(朱顺鹏);  Keshtegar B;  Qian GA(钱桂安);  Wang QY
Adobe PDF(2833Kb)  |  收藏  |  浏览/下载:410/287  |  提交时间:2020/08/26
Notch  Fatigue  Size effect  Failure probability  Life prediction  Weibull model  
Statistics of ceramic strength: Use ordinary Weibull distribution function or Weibull statistical fracture theory? 期刊论文
CERAMICS INTERNATIONAL, 2020, 卷号: 46, 期号: 13, 页码: 20751-20768
作者:  Lei, WS;  Zhang, PL;  Yu, ZS;  Qian GA(钱桂安)
Adobe PDF(4403Kb)  |  收藏  |  浏览/下载:213/86  |  提交时间:2020/09/07
Strength  Ceramics  Size effect  Weibull statistics  Ordinary Weibull distribution function  Weibull statistical fracture theory