IMECH-IR
(本次检索基于用户作品认领结果)

浏览/检索结果: 共31条,第1-10条 帮助

限定条件        
已选(0)清除 条数/页:   排序方式:
Defect induced cracking and modeling of fatigue strength for an additively manufactured Ti-6Al-4V alloy in very high cycle fatigue regime 期刊论文
THEORETICAL AND APPLIED FRACTURE MECHANICS, 2022, 卷号: 119, 页码: 10
作者:  Chi, Weiqian;  Wang, Wenjing;  Li, Ying;  Xu, Wei;  Sun CQ(孙成奇)
Adobe PDF(13675Kb)  |  收藏  |  浏览/下载:235/48  |  提交时间:2022/07/18
Very high cycle fatigue  Additively manufactured titanium alloy  Defect  Fatigue strength modeling  
Effects of defects on fatigue behavior of TC17 titanium alloy for compressor blades: Crack initiation and modeling of fatigue strength 期刊论文
ENGINEERING FRACTURE MECHANICS, 2022, 卷号: 259, 页码: 13
作者:  Chi, Weiqian;  Wang, Wenjing;  Xu, Wei;  Li, Gen;  Chen, Xin;  Sun CQ(孙成奇)
Adobe PDF(16769Kb)  |  收藏  |  浏览/下载:258/37  |  提交时间:2022/01/12
TC17 titanium alloy  Surface defect  Very high cycle fatigue  Crack initiation  Fatigue strength prediction  
Characteristic and mechanism of crack initiation and early growth of an additively manufactured Ti-6Al-4V in very high cycle fatigue regime 期刊论文
INTERNATIONAL JOURNAL OF MECHANICAL SCIENCES, 2021, 卷号: 205, 页码: 8
作者:  Sun CQ(孙成奇);  Chi, Weiqian;  Wang, Wenjing;  Duan, Yan
Adobe PDF(4522Kb)  |  收藏  |  浏览/下载:310/59  |  提交时间:2021/09/07
Very high cycle fatigue  Additively manufactured Ti-6Al-4V  Selective laser melting  Crack initiation mechanism  Grain refinement  
Effects of Notches and Defects on Dwell Fatigue Mechanism and Fatigue Life of Ti-6Al-4V ELI Alloy Used in Deep-Sea Submersibles 期刊论文
JOURNAL OF MARINE SCIENCE AND ENGINEERING, 2021, 卷号: 9, 期号: 8, 页码: 14
作者:  Sun J(孙健);  Wu, Lei;  Sun CQ(孙成奇)
Adobe PDF(5338Kb)  |  收藏  |  浏览/下载:309/116  |  提交时间:2021/11/01
titanium alloy Ti-6Al-4V ELI  notch  defect  dwell fatigue life  failure mechanism  
Fatigue endurance limit and crack front evolution in metallic glass 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2021, 卷号: 143, 页码: 9
作者:  Lei XQ(雷现奇);  袁力超o;  Peng, Liu;  Sun CQ(孙成奇);  Wei BC(魏炳忱);  Wei YJ(魏宇杰)
Adobe PDF(9123Kb)  |  收藏  |  浏览/下载:338/56  |  提交时间:2021/03/03
Fatigue endurance limit  Ultra-high cycle fatigue  Metallic glasses  Elliptical crack front  Stress intensity factor  
Crack initiation mechanism and fatigue life of titanium alloy Ti-6Al-2Sn-2Zr-3Mo-X: Effects of stress ratio and loading frequency 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 卷号: 798, 页码: 140265
作者:  Sun CQ(孙成奇);  Li YQ;  Huang RX;  Wang L;  Liu JL;  Zhou LL(周玲玲);  Duan GH(段桂花)
Adobe PDF(20240Kb)  |  收藏  |  浏览/下载:247/66  |  提交时间:2020/12/28
Ti-6Al-2Sn-2Zr-3Mo-X  HIGH-CYCLE FATIGUE  Stress ratio  TI-6AL-4V  Frequency  ALPHA  Crack initiation mechanism  BEHAVIOR  Fatigue life  FAILURE  MICROSTRUCTURE  STRENGTH  SIZE  
Mechanism of crack initiation and early growth of high strength steels in very high cycle fatigue regime 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 卷号: 771, 页码: 9
作者:  Song QY(宋清源);  Sun CQ(孙成奇)
Adobe PDF(3170Kb)  |  收藏  |  浏览/下载:421/80  |  提交时间:2020/03/11
very high cycle fatigue  High strength steels  Crack initiation mechanism  crack growth rate  Grain refinement  
试样疲劳性能尺度效应的概率控制体积方法 期刊论文
力学学报, 2019, 卷号: 51, 期号: 05, 页码: 1363-1371
作者:  李亚波;  宋清源;  杨凯;  陈一萍;  孙成奇;  洪友士
浏览  |  Adobe PDF(1382Kb)  |  收藏  |  浏览/下载:213/49  |  提交时间:2019/12/16
EA4T车轴钢  尺度效应  缺口效应  加载方式  疲劳强度  控制体积方法  
The formation of discontinuous gradient regimes during crack initiation in high strength steels under very high cycle fatigue 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2019, 卷号: 124, 页码: 483-492
作者:  Sun CQ(孙成奇);  Zhou LL(周玲玲);  Liu JL;  Wang Y(王垚);  Wu XL(武晓雷);  Wei YJ(魏宇杰)
浏览  |  Adobe PDF(8304Kb)  |  收藏  |  浏览/下载:322/133  |  提交时间:2019/09/09
Very high cycle fatigue  Gradient microstructure  Mechanism of crack initiation  Crack growth rate  
The behavior of crack initiation and early growth in high-cycle and very-high-cycle fatigue regimes for a titanium alloy 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2018, 卷号: 115, 期号: SI, 页码: 67-78
作者:  Pan XN(潘向南);  Su H(苏杭);  Sun CQ(孙成奇);  Hong YS(洪友士)
浏览  |  Adobe PDF(6409Kb)  |  收藏  |  浏览/下载:398/119  |  提交时间:2018/12/12
Very-high-cycle fatigue  Crack initiation  Mean stress  Titanium alloy  Equiaxed microstructure