A method for in situ measurement of the elastic behavior of a columnar thermal barrier coating 期刊论文
Acta Materialia, 2011, 卷号: 59, 期号: 9, 页码: 3612-3620
作者:  Eberl C;  Gianola DS;  Wang X;  He MY;  Evans AG;  Hemker KJ;  Eberl, C (reprint author), Karlsruhe Inst Technol, Inst Appl Mat, Karlsruhe, Germany
Adobe PDF(1162Kb)  |  收藏  |  浏览/下载:813/274  |  提交时间:2012/04/01
Thermal Barrier Coating (Tbc)  Digital Image Correlation  Elastic In Plane Modulus  Fracture Strain  Eb-pvd 7ysz  Residual-stresses  Microstructure  Indentation