| Crack initiation mechanisms under two stress ratios up to very-high-cycle fatigue regime for a selective laser melted Ti-6Al-4V 期刊论文 INTERNATIONAL JOURNAL OF FATIGUE, 2021, 卷号: 149, 页码: 10 Authors: Du LM(杜雷鸣); Pan XN(潘向南) ; Qian GA(钱桂安) ; Zheng L(郑亮); Hong YS(洪友士)
 Favorite  |  View/Download:57/0  |  Submit date:2021/08/03 Very-high-cycle fatigue Crack initiation mechanism Stress ratio Ti-6Al-4V Selective laser melting |
| Microstructure refinement and grain size distribution in crack initiation region of very-high-cycle fatigue regime for high-strength alloys 期刊论文 INTERNATIONAL JOURNAL OF FATIGUE, 2020, 卷号: 134, 页码: 12 Authors: Chang YK(常玉坤); Pan XN(潘向南) ; Zheng L; Hong YS(洪友士)
Adobe PDF(6646Kb)  |   Favorite  |  View/Download:133/27  |  Submit date:2020/05/18 Very-high-cycle fatigue Crack initiation Fine granular area (FGA) Rough area (RA) High-strength alloys |
| In-situ investigation on fatigue behaviors of Ti-6Al-4V manufactured by selective laser melting 期刊论文 INTERNATIONAL JOURNAL OF FATIGUE, 2020, 卷号: 133, 页码: 9 Authors: Qian GA(钱桂安) ; Jian ZM; Pan XN(潘向南) ; Berto F
Adobe PDF(2875Kb)  |   Favorite  |  View/Download:234/102  |  Submit date:2020/04/07 Selective laser melting In-situ SEM Ti-6Al-4V Low cycle fatigue Crack propagation |
| Characteristic of interior crack initiation and early growth for high cycle and very high cycle fatigue of a martensitic stainless steel 期刊论文 MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 卷号: 758, 页码: 112-120 Authors: 孙成奇i; Song QY(宋庆元); Zhou LL(周玲玲); Pan XN(潘向南)
Adobe PDF(5866Kb)  |   Favorite  |  View/Download:215/31  |  Submit date:2019/09/09 Very high cycle fatigue Crack initiation Crack growth rate Grain refinement Multi-site crack initiation |