IMECH-IR

浏览/检索结果: 共10条,第1-10条 帮助

限定条件                    
已选(0)清除 条数/页:   排序方式:
In-situ investigation on fatigue behaviors of Ti-6Al-4V manufactured by selective laser melting 会议论文
19th International Colloquium on Mechanical Fatigue of Metals (ICMFM), Univ Porto, Fac Engn, Porto, PORTUGAL, SEP 05-07, 2018
作者:  Qian GA(钱桂安);  Jian,Zhimo;  Pan XN(潘向南);  Berto,Filippo
Adobe PDF(2875Kb)  |  收藏  |  浏览/下载:106/37  |  提交时间:2022/11/24
Selective laser melting  In-situ SEM  Ti-6Al-4V  Low cycle fatigue  Crack propagation  
The behavior of crack initiation and early growth in high-cycle and very-high-cycle fatigue regimes for a titanium alloy 会议论文
4th IJFatigue and FFEMS Joint Workshop on Characterisation of Crack Tip Fields, Bonifacio, FRANCE, APR 10-12, 2017
作者:  Pan XN(潘向南);  Su H(苏杭);  Sun CQ(孙成奇);  Hong YS(洪友士)
浏览  |  Adobe PDF(6409Kb)  |  收藏  |  浏览/下载:377/61  |  提交时间:2019/04/19
Very-high-cycle fatigue  Crack initiation  Mean stress  Titanium alloy  Equiaxed microstructure  
The nature and the mechanism of crack initiation and early growth for very-high-cycle fatigue of metallic materials - An overview 会议论文
21st European Conference on Fracture (ECF), Catania, ITALY, JUN 20-24, 2016
作者:  Hong YS(洪友士);  Sun CQ(孙成奇);  Hong, YS (reprint author), Chinese Acad Sci, Inst Mech, LNM, Beijing 100190, Peoples R China.
浏览  |  Adobe PDF(7940Kb)  |  收藏  |  浏览/下载:336/150  |  提交时间:2018/01/16
High-strength Steels  Chromium-bearing Steel  Regime N-greater-than-10(7) Cycles  Severe Plastic-deformation  Ion Mass-spectrometry  Long-life Fatigue  Very-high-cycle Fatigue  Fatigue Crack Initiation  Fine-granular-area  Nanograins  High-strength Steels  Titanium Alloyss-n Curve  Ti-6al-4v Alloy  Propagation Mechanism  Ultrasonic Frequency  
Faceted crack initiation characteristics for high-cycle and very-high-cycle fatigue of a titanium alloy under different stress ratios 会议论文
5th International Conference on Crack Paths (CP), Ferrara, ITALY, SEP, 2015
作者:  Liu XL(刘小龙);  Sun CQ(孙成奇);  Hong YS(洪友士);  Hong, YS (reprint author), Chinese Acad Sci, Inst Mech, LNM, Beijing 100190, Peoples R China.
浏览  |  Adobe PDF(2579Kb)  |  收藏  |  浏览/下载:382/76  |  提交时间:2017/05/12
Ti-6al-4v Alloy  Faceted Crack Initiation  Very-high-cycle Fatigue  Stress Ratio  Cluster Of Primary Alpha Grains  Competing Failure Modes  Poisson Defect Statistics  Ti-6al-4v Alloy  Structural-materials  Mean Stress  Strength  Microstructure  Behavior  Duality  Surface  
The formation mechanism of characteristic region at crack initiation for very-high-cycle fatigue of high-strength steels 会议论文
3rd International Conference on Characterisation of Crack Tip Fields, Urbino, ITALY, APR 20-22, 2015
作者:  Hong YS(洪友士);  Liu XL(刘小龙);  Lei ZQ(雷铮强);  Sun CQ(孙成奇);  Hong, YS (reprint author), Chinese Acad Sci, Inst Mech, LNM, Beijing 100190, Peoples R China.
浏览  |  Adobe PDF(3960Kb)  |  收藏  |  浏览/下载:337/107  |  提交时间:2017/05/12
Very-high-cycle Fatigue  Fatigue Crack Initiation  Fine-granular-area  Nanograins  High-strength Steels  Chromium-bearing Steel  Long-life Fatigue  N-greater-than-10(7) Cycles  Residual-stresses  Vhcf-regime  Behavior  Inclusions  Propagation  Damage  Size  
Experimental Investigation of Dynamic Fracture Behaviors of Polymethyl Methacrylate 会议论文
23rd World Forum on Advanced Polymeric Materials (POLYCHAR), Univ Nebraska Lincoln, Lincoln, NE, MAY 11-15, 2015
作者:  Gao GY;  Zhou J;  Li Z;  Li, Z (reprint author), Peking Univ, State Key Lab Turbulence & Complex Syst, Beijing 100871, Peoples R China.;  Li, Z (reprint author), Peking Univ, Coll Engn, Beijing 100871, Peoples R China.
浏览  |  Adobe PDF(2033Kb)  |  收藏  |  浏览/下载:249/104  |  提交时间:2017/05/12
Crack Interaction  Fracture  Optical Method Of Caustics  Semi-circular Bending  Toughness  Stress Intensity Factor  Semicircular Bend Technique  Crack-propagation  Brittle-fracture  Caustic Analysis  Specimen  Pmma  Parallel  Field  Rock  
Reliability analysis of very-high-cycle fatigue crack initiation for a high strength steel 会议论文
International Conference on Airworthiness & Fatigue-7th ICSAELS Series Conference, 中国北京/Beijing, China, 2013-03-25
作者:  Lei ZQ(雷铮强);  Xie JJ(谢季佳);  Sun CQ(孙成奇);  Liu XL;  Hong YS(洪友士)
浏览  |  Adobe PDF(47Kb)  |  收藏  |  浏览/下载:479/109  |  提交时间:2014/04/02
Steel  Fatigue  Initiation  Strength  Crack  Analysis  Cycle  
Investigation on the effect of crack length on mechanical properties of functionally graded materials 会议论文
2010 International Conference on Frontiers of Manufacturing and Design Science, ICFMD2010, Chongqing, China, DEC 11-12, 2010
作者:  Chen G;  Zhao XY(赵希宇);  Zhai PC
Adobe PDF(291Kb)  |  收藏  |  浏览/下载:577/139  |  提交时间:2013/02/26
Coatings  Cracks  Creep  Finite Element Method  Human Engineering  Manufacture  Mechanical Properties  Stress Intensity Factors  Thermal Barrier Coatings  Crack Length  Crack Tip Fields  Finite Element  Functionally Graded  Maximum Displacement  Numerical Results  Principal Stress  Pure Metals  Stress Intensity  Thermal Barrier  Thermo-mechanical  Work Environments  
Correlation of Crack Initiation Parameters with Life Estimation for Very-High-Cycle Fatigue of High Strength Steels 会议论文
第18届国际计算与实验科学工程大会(International Conference on Computational and Experimental Engineering and Scinece)(ICCES’2011), Nanjing, China, April 18-21, 2011
作者:  Hong YS(洪友士);  Sun CQ(孙成奇);  Zhao AG(赵爱国);  Youshi Hong
Adobe PDF(35Kb)  |  收藏  |  浏览/下载:876/231  |  提交时间:2013/03/11
Very-high-cycle Fatigue  High Strength Steels  Crack Initiation  Fatigue Life Estimation  Fga  
Effect of Aqueous Environment on High Cycle and Very-High-Cycle Fatigue Behavior for a Structural Steel 会议论文
8th International Conference on Fracture and Strength of Solids (FEOFS) 2010, Kuala Lumpur, MALAYSIA, JUN 07-09, 2010
作者:  Hong YS(洪友士);  Qian GA(钱桂安);  Hong, YS (reprint author), Chinese Acad Sci, Inst Mech, LNM, Beijing 100190, Peoples R China
浏览  |  Adobe PDF(2756Kb)  |  收藏  |  浏览/下载:977/159  |  提交时间:2012/04/01
Very-high-cycle Fatigue  Aqueous Environment  Fatigue Strength  Fatigue Crack Initiation  Fatigue Crack Propagation  Structural Steel  High-strength Steels  Crack-propagation  Initiation  Fracture