Fatigue Behavior of Inorganic-Organic Hybrid "Lunar Cement" 期刊论文
SCIENTIFIC REPORTS, 2019, 卷号: 9, 页码: AR002238
Authors:  Su H(苏杭);  Hong YS(洪友士);  Chen TH;  Kou R;  Wang M;  Zhong Y;  Qiao Y
Favorite  |  View/Download:11/0  |  Submit date:2019/04/11
The behavior of crack initiation and early growth in high-cycle and very-high-cycle fatigue regimes for a titanium alloy 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2018, 卷号: 115, 期号: SI, 页码: 67-78
Authors:  Pan XN(潘向南);  Su H(苏杭);  Sun CQ(孙成奇);  Hong YS(洪友士)
View  |  Adobe PDF(6409Kb)  |  Favorite  |  View/Download:22/4  |  Submit date:2018/12/12
Very-high-cycle fatigue  Crack initiation  Mean stress  Titanium alloy  Equiaxed microstructure  
The behavior of crack initiation and early growth in high-cycle and very-high-cycle fatigue regimes for a titanium alloy 会议论文
4th IJFatigue and FFEMS Joint Workshop on Characterisation of Crack Tip Fields, Bonifacio, FRANCE, APR 10-12, 2017
Authors:  Pan XN(潘向南);  Su H(苏杭);  Sun CQ(孙成奇);  Hong YS(洪友士)
View  |  Adobe PDF(6409Kb)  |  Favorite  |  View/Download:16/2  |  Submit date:2019/04/19
Very-high-cycle fatigue  Crack initiation  Mean stress  Titanium alloy  Equiaxed microstructure  
Error reduction for time-resolved PIV data based on Navier-Stokes equations 期刊论文
EXPERIMENTS IN FLUIDS, 2018, 卷号: 59, 期号: 10, 页码: 149
Authors:  Wang HP(王洪平);  Gao Q;  Wang SZ(王士召);  Li YH;  Wang ZY;  Wang JJ
View  |  Adobe PDF(8525Kb)  |  Favorite  |  View/Download:28/4  |  Submit date:2018/10/30
一种用于疲劳强度测试的并行分支升降法 专利
发明专利. 一种用于疲劳强度测试的并行分支升降法, 专利号: ZL201610237687.X, 申请日期: 2016-04-15, 授权日期: 2018-08-10
Inventors:  洪友士;  姜青青;  孙成奇;  谢季佳
View  |  Adobe PDF(673Kb)  |  Favorite  |  View/Download:31/4  |  Submit date:2018/12/05
Crack growth rates and microstructure feature of initiation region for very-high-cycle fatigue of a high-strength steel 期刊论文
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2018, 卷号: 41, 期号: 8, 页码: 1717-1732
Authors:  Hu YP(胡远培);  Sun CQ(孙成奇);  Hong YS(洪友士)
View  |  Adobe PDF(2025Kb)  |  Favorite  |  View/Download:14/4  |  Submit date:2018/10/30
crack growth rate  crack initiation  fine-granular-area  high-strength steel  variable amplitude loading  very-high-cycle fatigue  
Effects of Loading Frequency and Loading Type on High-Cycle and Very-High-Cycle Fatigue of a High-Strength Steel 期刊论文
MATERIALS, MATERIALS, 2018, 2018, 卷号: 11, 11, 期号: 8, 页码: 1456, 1456
Authors:  Hu YP(胡远培);  Sun CQ(孙成奇);  Xie JJ(谢季佳);  Hong YS(洪友士)
View  |  Adobe PDF(2130Kb)  |  Favorite  |  View/Download:24/5  |  Submit date:2018/10/30
loading frequency  loading frequency  loading type  loading type  very-high-cycle fatigue  very-high-cycle fatigue  fatigue strength  fatigue strength  high-strength steel  high-strength steel  
水分解微推力器脉冲燃烧过程实验研究 期刊论文
推进技术, 2018, 卷号: 39, 期号: 4, 页码: 843-848
Authors:  攸兴杰;  沈岩;  余西龙;  李飞;  卢国权
View  |  Adobe PDF(1353Kb)  |  Favorite  |  View/Download:33/6  |  Submit date:2018/10/24
微推进  水分解推力器  氢氧混合气体  定容燃烧  
野外斜坡地表入渗性能与渗透系数测量方法与装置 专利
发明专利. 野外斜坡地表入渗性能与渗透系数测量方法与装置, 专利号: ZL201410613641.4, 申请日期: 2014-11-05, 授权日期: 2018-02-23
Inventors:  史鹏飞;  吴梦喜;  程鹏达;  程瑞林;  慕洪友;  何福娟;  苏鹏;  张斌;  邱焕峰
View  |  Adobe PDF(612Kb)  |  Favorite  |  View/Download:32/4  |  Submit date:2019/01/04
预测试样尺寸对疲劳寿命影响的方法 专利
发明专利. 预测试样尺寸对疲劳寿命影响的方法, 专利号: ZL201610059873.9, 申请日期: 2016-01-28, 授权日期: 2018-02-16
Inventors:  洪友士;  孙成奇;  刘小龙