Fatigue endurance limit and crack front evolution in metallic glass 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2021, 卷号: 143, 页码: 9
Authors:  Lei XQ(雷现奇);  袁力超o;  Peng, Liu;  Sun CQ(孙成奇);  Wei BC(魏炳忱);  Wei YJ(魏宇杰)
Adobe PDF(9123Kb)  |  Favorite  |  View/Download:374/60  |  Submit date:2021/03/03
Fatigue endurance limit  Ultra-high cycle fatigue  Metallic glasses  Elliptical crack front  Stress intensity factor  