Nanograin layer formation at crack initiation region for very-high-cycle fatigue of a Ti-6Al-4V alloy 期刊论文
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2017, 卷号: 40, 期号: 6, 页码: 979-993
Authors:  Su H(苏杭);  Liu XL(刘小龙);  Sun CQ(孙成奇);  Hong YS(洪友士)
View  |  Adobe PDF(1106Kb)  |  Favorite  |  View/Download:341/123  |  Submit date:2017/10/27
Crack Initiation  Fatigue Life  Nanograins  Ti-6al-4v Alloy  Very-high-cycle Fatigue  
S38C车轴钢的旋转弯曲和超声振动疲劳性能 期刊论文
润滑与密封, 2017, 卷号: 42, 期号: 03, 页码: 124-128+140
Authors:  李亚波;  杨凯;  陈一萍;  姜青青;  孙成奇;  洪友士
View  |  Adobe PDF(2608Kb)  |  Favorite  |  View/Download:322/91  |  Submit date:2017/12/22
S38c钢  旋转弯曲  超声振动  疲劳性能