已选(0)清除
条数/页: 排序方式: |
| On the microstructure evolution of a nuclear-use steel after heavy ion irradiation 会议论文 3rd International Conference on Chemistry and Energy Research, ICCER 2020, 广东深圳, 23 October 2020 到 25 October 2020 作者: Song L; Ye F; Li JH(李江华); Ma X; Zhang R; Qiu S; Liu X Adobe PDF(3670Kb)  |  收藏  |  浏览/下载:129/35  |  提交时间:2021/11/30 |
| Plasticity performance of Al0.5CoCrCuFeNi high-entropy alloys under nanoindentation 会议论文 17th IUMRS International Conference in Asia, Qingdao, PEOPLES R CHINA, OCT 20-24, 2016 作者: Yu LP; Chen SY; Ren JL; Ren Y; Yang FQ; Dahmen KA; Liaw PK; Ren, JL (reprint author), Zhengzhou Univ, Sch Math & Stat, Zhengzhou 150001, Henan, Peoples R China. 浏览  |  Adobe PDF(958Kb)  |  收藏  |  浏览/下载:238/73  |  提交时间:2018/01/16 Time-series Cryogenic Temperatures Multicomponent Alloys Serration Behavior Strange Attractors Metallic Glasses Fatigue Behavior Flow High-entropy Alloys Nanoindentation Critical Behavior Chaotic Behaviordeformation Dimension |
| Effect of laser shock peening on the surface morphology of metallic glasses 会议论文 17th IUMRS International Conference in Asia, IUMRS-ICA 2016, Qingdao, China, October 20, 2016 - October 24, 2016 作者: Li YS; Zhang K(张坤); Duan GH(段桂花); Xu GY(徐光跃); Wei YH; Wei YP(魏延鹏); Wei BC(魏炳忱) 浏览  |  Adobe PDF(873Kb)  |  收藏  |  浏览/下载:358/88  |  提交时间:2018/11/08 Glass Metals Morphology Surface morphology Amorphous systems Crystalline degree Effective approaches Laser shock peening Localized structures Morphology evolution Shaped structures Zr based metallic glass |
| 压头形状和表面梯度层对纳米硬度测量的影响 会议论文 北京力学会第21届学术年会暨北京振动工程学会第22届学术年会, 中国北京, 2015-01-11 作者: 张群; 杨荣; 肖攀; 白以龙 浏览  |  Adobe PDF(564Kb)  |  收藏  |  浏览/下载:214/53  |  提交时间:2016/08/16 纳米压入 纳米硬度 表面梯度层 压头几何形状 尺寸效应 |
| Experimental study of the influence of thermal shock on mechanical properties of ceramic coating systems 会议论文 13th International Conference on Fracture 2013, ICF 2013, Beijing, China, June 16, 2013 - June 21, 2013 作者: Li XN(李霄娜); Liang LH(粱立红); Wei H; Wei YG(魏悦广) 浏览  |  Adobe PDF(683Kb)  |  收藏  |  浏览/下载:244/77  |  提交时间:2018/11/08 Bending strength Bending tests Ceramic coatings Ceramic materials Elastic moduli Fracture Hardness Mechanical properties Microstructure Thermal shock Air plasma sprayed Change of temperatures Coating substrate systems Nanoindentation tests Nanostructured coatings Shock temperature Temperature range Three point bending test |
| Contact and Friction of One- and Two-Dimensional Nanostructures 会议论文 作者: Zhang Y(张吟); Zhao YP(赵亚溥) 浏览  |  Adobe PDF(671Kb)  |  收藏  |  浏览/下载:831/427  |  提交时间:2014/03/04 |
| A New Elastic-Plastic Model for Describing the Nanoindentation Size Effects of Surface-Nanocrystalline Materials 会议论文 The 23rd International Congress of Theoretical and Applied Mechanics (ICTAM2012), Beijing, China., 19-24 August, 2012 作者: Yu SM(于韶明); Wei YG(魏悦广) Adobe PDF(83Kb)  |  收藏  |  浏览/下载:575/143  |  提交时间:2013/03/05 |
| Approaches to remove size effect due to indenter roundness in nano-indentation 会议论文 23rd International Congress of Theoretical and Applied Mechanics, 中国北京/Beijing, China, 2012-08-19 作者: Yang R(杨荣); Zhang TH(张泰华); Zhang Q(张群); Bai YL(白以龙) 浏览  |  Adobe PDF(188Kb)  |  收藏  |  浏览/下载:486/137  |  提交时间:2014/04/02 Indentation Roundness Indenter Remove Abrasion Effect Material Interpret Within Results Hundred Exist During |
| Correction of shear creep compliance determined by conical indentation 会议论文 23rd International Congress of Theoretical and Applied Mechanics, 中国北京/Beijing, China, 2012-08-19 作者: Peng GJ(彭光健); Zhang TH(张泰华); Feng YH(冯义辉) 浏览  |  Adobe PDF(81Kb)  |  收藏  |  浏览/下载:432/124  |  提交时间:2014/04/02 Indentation Creep Conical Shear Compliance Determined Angle Uniaxial Large Smaller Relaxation Determination Ratio Theoret Tension Result Error Found Poisson Equal |
| Intrinsic lengths govern failure mode transition in metallic glasses 会议论文 ICTAM, 北京, 2012-8 作者: Dai LH(戴兰宏); Chen Y(陈艳) Adobe PDF(691Kb)  |  收藏  |  浏览/下载:1779/1224  |  提交时间:2013/03/01 |