Shattered rim and shelling of high-speed railway wheels in the very-high-cycle fatigue regime under rolling contact loading 期刊论文
ENGINEERING FAILURE ANALYSIS, 2019, 卷号: 97, 页码: 556-567
作者:  Cong T;  Han JM;  Hong YS(洪友士);  Domblesky JP;  Liu XL(刘小龙)
浏览  |  Adobe PDF(3595Kb)  |  收藏  |  浏览/下载:294/77  |  提交时间:2019/04/11
High-speed railway wheel  Shattered rim  Shelling  Very-high-cycle fatigue  Rolling contact loading  Crack initiation  
Nanograin layer formation at crack initiation region for very-high-cycle fatigue of a Ti-6Al-4V alloy 期刊论文
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2017, 卷号: 40, 期号: 6, 页码: 979-993
作者:  Su H(苏杭);  Liu XL(刘小龙);  Sun CQ(孙成奇);  Hong YS(洪友士)
浏览  |  Adobe PDF(1106Kb)  |  收藏  |  浏览/下载:327/118  |  提交时间:2017/10/27
Crack Initiation  Fatigue Life  Nanograins  Ti-6al-4v Alloy  Very-high-cycle Fatigue  
Faceted crack initiation characteristics for high-cycle and very-high-cycle fatigue of a titanium alloy under different stress ratios 会议论文
5th International Conference on Crack Paths (CP), Ferrara, ITALY, SEP, 2015
作者:  Liu XL(刘小龙);  Sun CQ(孙成奇);  Hong YS(洪友士);  Hong, YS (reprint author), Chinese Acad Sci, Inst Mech, LNM, Beijing 100190, Peoples R China.
浏览  |  Adobe PDF(2579Kb)  |  收藏  |  浏览/下载:381/76  |  提交时间:2017/05/12
Ti-6al-4v Alloy  Faceted Crack Initiation  Very-high-cycle Fatigue  Stress Ratio  Cluster Of Primary Alpha Grains  Competing Failure Modes  Poisson Defect Statistics  Ti-6al-4v Alloy  Structural-materials  Mean Stress  Strength  Microstructure  Behavior  Duality  Surface  
Very-high-cycle fatigue behavior of a structural steel with and without induced surface defects 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2016, 卷号: 93, 期号: 2, 页码: 352-362
作者:  Jiang QQ;  Sun CQ(孙成奇);  Liu XL(刘小龙);  Hong YS(洪友士);  Hong, YS (reprint author), Chinese Acad Sci, Inst Mech, LNM, Beijing 100190, Peoples R China.
浏览  |  Adobe PDF(3394Kb)  |  收藏  |  浏览/下载:225/85  |  提交时间:2016/12/08
Very-high-cycle Fatigue  Surface Defect  Fine-granular-area  Crack Initiation  Structural Steel  
Faceted crack initiation characteristics for high-cycle and very-high-cycle fatigue of a titanium alloy under different stress ratios 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2016, 卷号: 92, 期号: 2, 页码: 434-441
作者:  Liu XL(刘小龙);  Sun CQ(孙成奇);  Hong YS(洪友士);  Hong, YS (reprint author), Chinese Acad Sci, Inst Mech, LNM, Beijing 100190, Peoples R China.
浏览  |  Adobe PDF(2579Kb)  |  收藏  |  浏览/下载:265/109  |  提交时间:2016/12/08
Ti-6al-4v Alloy  Faceted Crack Initiation  Very-high-cycle Fatigue  Stress Ratio  Cluster Of Primary Alpha Grains  
The formation mechanism of characteristic region at crack initiation for very-high-cycle fatigue of high-strength steels 会议论文
3rd International Conference on Characterisation of Crack Tip Fields, Urbino, ITALY, APR 20-22, 2015
作者:  Hong YS(洪友士);  Liu XL(刘小龙);  Lei ZQ(雷铮强);  Sun CQ(孙成奇);  Hong, YS (reprint author), Chinese Acad Sci, Inst Mech, LNM, Beijing 100190, Peoples R China.
浏览  |  Adobe PDF(3960Kb)  |  收藏  |  浏览/下载:336/107  |  提交时间:2017/05/12
Very-high-cycle Fatigue  Fatigue Crack Initiation  Fine-granular-area  Nanograins  High-strength Steels  Chromium-bearing Steel  Long-life Fatigue  N-greater-than-10(7) Cycles  Residual-stresses  Vhcf-regime  Behavior  Inclusions  Propagation  Damage  Size  
Effects of stress ratio on high-cycle and very-high-cycle fatigue behavior of a Ti-6Al-4V alloy 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 卷号: 622, 页码: 228-235
作者:  Liu XL(刘小龙);  Sun CQ(孙成奇);  Hong YS(洪友士);  Hong, YS (reprint author), Chinese Acad Sci, Inst Mech, State Key Lab Nonlinear Mech, Beijing 100190, Peoples R China.
浏览  |  Adobe PDF(3165Kb)  |  收藏  |  浏览/下载:392/115  |  提交时间:2015/03/17
Ti-6al-4v Alloy  Stress Ratio  Crack Initiation Type  Crack Growth Threshold  Very-high-cycle Fatigue