Faceted crack initiation characteristics for high-cycle and very-high-cycle fatigue of a titanium alloy under different stress ratios 会议论文
5th International Conference on Crack Paths (CP), Ferrara, ITALY, SEP, 2015
作者:  Liu XL(刘小龙);  Sun CQ(孙成奇);  Hong YS(洪友士);  Hong, YS (reprint author), Chinese Acad Sci, Inst Mech, LNM, Beijing 100190, Peoples R China.
浏览  |  Adobe PDF(2579Kb)  |  收藏  |  浏览/下载:389/79  |  提交时间:2017/05/12
Ti-6al-4v Alloy  Faceted Crack Initiation  Very-high-cycle Fatigue  Stress Ratio  Cluster Of Primary Alpha Grains  Competing Failure Modes  Poisson Defect Statistics  Ti-6al-4v Alloy  Structural-materials  Mean Stress  Strength  Microstructure  Behavior  Duality  Surface  
A two-parameter model to predict fatigue life of high-strength steels in a very high cycle fatigue regime 期刊论文
ACTA MECHANICA SINICA, 2015, 卷号: 31, 期号: 3, 页码: 383-391
作者:  Sun CQ(孙成奇);  Liu XL(刘小龙);  Hong YS(洪友士)
浏览  |  Adobe PDF(1387Kb)  |  收藏  |  浏览/下载:357/113  |  提交时间:2015/07/16
Very High-cycle Fatigue  High-strength Steels  Fatigue Life  Inclusion Size  Crack Growth Rate  
Effects of stress ratio on crack growth rate and fatigue strength for high cycle and very-high-cycle fatigue of metallic materials 期刊论文
Mechanics of Materials, 2014, 卷号: 69, 期号: 1, 页码: 227-236
作者:  Sun CQ(孙成奇);  Lei ZQ(雷铮强);  Hong YS(洪友士);  Hong, YS (reprint author), Chinese Acad Sci, Inst Mech, State Key Lab Nonlinear Mech, Beijing 100190, Peoples R China.
浏览  |  Adobe PDF(913Kb)  |  收藏  |  浏览/下载:760/268  |  提交时间:2014/05/09
Surface Hardness  Sulfate Attack  Concrete  Damage Evolution  
Effects of inclusion size and stress ratio on fatigue strength for high-strength steels with fish-eye mode failure 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2013, 卷号: 48, 页码: 19-27
作者:  Sun CQ(孙成奇);  Lei ZQ(雷铮强);  Xie JJ(谢季佳);  Hong YS(洪友士);  Hong, YS (reprint author), Chinese Acad Sci, State Key Lab Nonlinear Mech, Inst Mech, Beijing 100190, Peoples R China.
Adobe PDF(805Kb)  |  收藏  |  浏览/下载:1720/500  |  提交时间:2013/04/07
Very-high-cycle Fatigue  Inclusion Size  Stress Ratio  Fatigue Strength  High-strength Steels  
A cumulative damage model for fatigue life estimation of high-strength steels in high-cycle and very-high-cycle fatigue regimes 期刊论文
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2012, 卷号: 35, 期号: 7, 页码: 638-647
作者:  Sun CQ(孙成奇);  Xie JJ(谢季佳);  Zhao AG(赵爱国);  Lei ZQ(雷铮强);  Hong YS(洪友士);  Hong, Y;  Chinese Acad Sci, State Key Lab Nonlinear Mech, Inst Mech, Beijing 100190, Peoples R China.
Adobe PDF(909Kb)  |  收藏  |  浏览/下载:1033/309  |  提交时间:2013/01/18
Crack Growth Rate  Fatigue Damage  Fish-eye Fracture  High-cycle Fatigue  Very-high-cycle Fatigue  Life Estimation  Subsurface Crack Initiation  Chromium Bearing Steel  S-n Curve  Gigacycle Fatigue  Part i  Mechanism  Behavior  Failure  Inclusions  Size  
Correlation of crack growth rate and stress ratio for fatigue damage containing very high cycle fatigue regime 期刊论文
THEORETICAL & APPLIED MECHANICS LETTERS, 2012, 卷号: 2, 期号: 3, 页码: 031004
作者:  Sun CQ(孙成奇);  Hong YS(洪友士)
Adobe PDF(392Kb)  |  收藏  |  浏览/下载:637/177  |  提交时间:2013/01/16
Very High Cycle Fatigue  Crack Growth Rate  Stress Ratio  Fatigue Strength  
Axisymmetric compressive buckling of multi-walled carbon nanotubes under different boundary conditions 期刊论文
ACTA MECHANICA SINICA, 2012, 卷号: 28, 期号: 1, 页码: 83-90
作者:  Sun CQ(孙成奇);  Liu KX;  Hong YS(洪友士);  Sun, CQ;  Chinese Acad Sci, Inst Mech, State Key Lab Nonlinear Mech, Beijing 100190, Peoples R China.
Adobe PDF(438Kb)  |  收藏  |  浏览/下载:715/197  |  提交时间:2013/01/18
Carbon Nanotube  Buckling  Van Der Waals Forces  Elastic Medium  High-pressure  Shell  Deformation  Instability  Behavior