Crack initiation mechanisms under two stress ratios up to very-high-cycle fatigue regime for a selective laser melted Ti-6Al-4V 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2021, 卷号: 149, 页码: 10
作者:  Du LM(杜雷鸣);  Pan XN(潘向南);  Qian GA(钱桂安);  Zheng L(郑亮);  Hong YS(洪友士)
Adobe PDF(14294Kb)  |  收藏  |  浏览/下载:290/55  |  提交时间:2021/08/03
Very-high-cycle fatigue  Crack initiation mechanism  Stress ratio  Ti-6Al-4V  Selective laser melting  
S38C车轴表层梯度材料的疲劳裂纹扩展性能研究 期刊论文
润滑与密封, 2021, 卷号: 46, 期号: 04, 页码: 106-110
作者:  邹洪伟;  李亚波;  马丽英;  洪友士
Adobe PDF(829Kb)  |  收藏  |  浏览/下载:198/52  |  提交时间:2021/08/25
S38C  三点弯曲  残余应力  裂纹扩展特性  
Nanograin formation in dimple ridges due to local severe-plastic-deformation during ductile fracture 期刊论文
Scripta Materialia, 2021, 卷号: 194, 页码: 113631
作者:  Pan XN(潘向南);  Qian GA(钱桂安);  Hong YS(洪友士)
Adobe PDF(2120Kb)  |  收藏  |  浏览/下载:517/119  |  提交时间:2020/11/23
nanograins  ductile fracture  dimple ridge  severe plastic deformation (SPD)  titanium alloy  
Influence of processing parameters of selective laser melting on high-cycle and very-high-cycle fatigue behaviour of Ti-6Al-4V 期刊论文
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2020, 页码: 17
作者:  Du LM(杜雷鸣);  Qian GA(钱桂安);  Zheng L;  Hong YS(洪友士)
Adobe PDF(52217Kb)  |  收藏  |  浏览/下载:309/101  |  提交时间:2020/11/30
orthogonal experiment design  processing parameters  selective laser melting  Ti-6Al-4V  very-high-cycle fatigue  
The mechanism of internal fatigue-crack initiation and early growth in a titanium alloy with lamellar and equiaxed microstructure 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 卷号: 798, 页码: 140110
作者:  Pan XN(潘向南);  Xu SW(徐守文);  Qian GA(钱桂安);  Alexander N;  Andrey S;  Thierry PL;  Hong YS(洪友士)
Adobe PDF(27976Kb)  |  收藏  |  浏览/下载:520/99  |  提交时间:2020/08/26
Microstructure refinement and grain size distribution in crack initiation region of very-high-cycle fatigue regime for high-strength alloys 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2020, 卷号: 134, 页码: 12
作者:  Chang YK(常玉坤);  Pan XN(潘向南);  Zheng L;  Hong YS(洪友士)
Adobe PDF(6646Kb)  |  收藏  |  浏览/下载:306/112  |  提交时间:2020/05/18
Very-high-cycle fatigue  Crack initiation  Fine granular area (FGA)  Rough area (RA)  High-strength alloys  
Shattered rim and shelling of high-speed railway wheels in the very-high-cycle fatigue regime under rolling contact loading 期刊论文
ENGINEERING FAILURE ANALYSIS, 2019, 卷号: 97, 页码: 556-567
作者:  Cong T;  Han JM;  Hong YS(洪友士);  Domblesky JP;  Liu XL(刘小龙)
浏览  |  Adobe PDF(3595Kb)  |  收藏  |  浏览/下载:296/78  |  提交时间:2019/04/11
High-speed railway wheel  Shattered rim  Shelling  Very-high-cycle fatigue  Rolling contact loading  Crack initiation  
Fatigue Behavior of Inorganic-Organic Hybrid "Lunar Cement" 期刊论文
SCIENTIFIC REPORTS, 2019, 卷号: 9, 页码: AR002238
作者:  Su H(苏杭);  Hong YS(洪友士);  Chen TH;  Kou R;  Wang M;  Zhong Y;  Qiao Y
浏览  |  Adobe PDF(2835Kb)  |  收藏  |  浏览/下载:227/41  |  提交时间:2019/04/11
The behavior of crack initiation and early growth in high-cycle and very-high-cycle fatigue regimes for a titanium alloy 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2018, 卷号: 115, 期号: SI, 页码: 67-78
作者:  Pan XN(潘向南);  Su H(苏杭);  Sun CQ(孙成奇);  Hong YS(洪友士)
浏览  |  Adobe PDF(6409Kb)  |  收藏  |  浏览/下载:403/122  |  提交时间:2018/12/12
Very-high-cycle fatigue  Crack initiation  Mean stress  Titanium alloy  Equiaxed microstructure  
The behavior of crack initiation and early growth in high-cycle and very-high-cycle fatigue regimes for a titanium alloy 会议论文
4th IJFatigue and FFEMS Joint Workshop on Characterisation of Crack Tip Fields, Bonifacio, FRANCE, APR 10-12, 2017
作者:  Pan XN(潘向南);  Su H(苏杭);  Sun CQ(孙成奇);  Hong YS(洪友士)
浏览  |  Adobe PDF(6409Kb)  |  收藏  |  浏览/下载:378/61  |  提交时间:2019/04/19
Very-high-cycle fatigue  Crack initiation  Mean stress  Titanium alloy  Equiaxed microstructure